N. Volz, F. Xue, C. H. Zenk, et al. Understanding creep of a single-crystalline Co-Al-W-Ta superalloy by studying the deformation mechanism, segregation tendency and stacking fault energy Acta Materialia 214 117019 (2021) abstract